| Characterization | Size | Temperature Of Materials Carried | Belt Surfac Temperature Temperatura |
| Coke | 100-200mm(4-8inch) | 70-100℃ | 50-60℃ |
| Cement | Power/Polvo | 200-250℃ | 80-90℃ |
| ClinkerLa | 10-30mm(0.4-1.2inch) | 100-220℃ | 100-110℃ |
| Molding | - | 200-250℃ | 80-90℃ |
| Metal Powder | - | 120℃ | 120-130℃ |
| Raw Material | (30mm(1.2inch)) | 180-220℃ | 100-120℃ |
| Sintered Ore | 25-200mm(1-8inch) | 200-400℃ | 130-150℃ |
| Return Of Sintered Ore | (10mm(0.4inch)) | 260℃ | 180-200℃ |
| Physical property indexes | Execution standard:GB/T20021-2005 | |||||
| Item | Test temperature | |||||
| ≤ 125°C | ≤ 150°C | ≤ 200°C(EPDM) | ≤ 300C(EPDM) | |||
| Change range allowed | ||||||
| Hardness | The difference between the formerafter the aging | +20 | ±20 | ±20 | ±20 | |
| The maximum value after aging | 85 | 85 | 85 | 85 | ||
| The tensile strength | The performance rate/% | -30 | -40 | -40 | -40 | |
| After aging the lowest Mpa | 10 | 5 | 5 | 5 | ||
| Tensile elongation | After aging rate/% | -50 | -55 | -55 | -55 | |
| After aging the lowest /% | 200 | 180 | 180 | 180 | ||
| Belt Type Material | Fabric Typ | Single Fabric Strength(N/mm) | Single Fabric Thickness(mm) | Cover Thickness(mm) | No.Of Ply | Belt Width Range(mm) | Belt Length(m)Roll | ||
| Top | Bottom | ||||||||
Nylon(NN) Belt/ | NN100 | 100 | 1 | 2-25 | 0-10 | 2-10 | 300-2200 | 2-650 | |
| NN125 | 125 | 1.05 | |||||||
| NN150 | 150 | 1.1 | |||||||
| NN200 | 200 | 1.2 | |||||||
| NN250 | 250 | 1.4 | |||||||
| NN300 | 300 | 1.6 | |||||||
| NN400 | 400 | 2.2 | |||||||
Polyester Belt/ | EP100 | 100 | 1 | 2-25 | 0-10 | 2-8 | 300-2200 | 2-650 | |
| EP125 | 125 | 1.05 | |||||||
| EP150 | 150 | 1.1 | |||||||
| EP160 | 175 | 1.15 | |||||||
| EP200 | 200 | 1.2 | |||||||
| EP250 | 250 | 1.4 | |||||||
| EP300 | 300 | 1.6 | |||||||
| EP350 | 350 | 1.8 | |||||||
| EP400 | 400 | 2.2 | |||||||
| Cotton Belt/ | CC-56 | 56 | 1.10 | 2-25 | 0-10 | 3-12 | 300-2200 | 2-50 | |
| Design Code | DIN22102 ref | Characterization | Tensile in Mpa | Elongation in % | Abrasion in mm³ | Hardness in SHA | |||
| HS EPY | Y | High Abrasion Resistance | ≥20 | ≥400 | ≤150 | 60±5 | |||
| HS EPX | X | Resistance to Cutting | ≥25 | ≥450 | ≤120 | 60±5 | |||
| HS EPW | W | Extra Abrasion Resistance | ≥18 | ≥450 | ≤90 | 60±5 | |||
| HS EPZ | Z | Abrasion Resistance | ≥15 | ≥350 | ≤250 | 60±5 | |||
| HS EPKY | K,Y | Flame retardant | ≥20 | ≥400 | ≤150 | 60±5 | |||
| HS EPSY | S,Y | Flame retardant | ≥20 | ≥400 | ≤150 | 60±5 | |||
| HS EPK | K | Flame retardant | ≥15 | ≥350 | ≤150 | 60±5 | |||
| HS EPS | S | Flame retardant | ≥15 | ≥350 | ≤150 | 60±5 | |||
| Design Code | DIN22102 ref | Cover Properties of Special Characterization | EP conveyor belt Tensile in Mpa | Elongation in % | Abrasion in mm³ | Base material | |||
| HS EPOR | G | Oil Resistant -30 °C ~+125°C | ≥15 | ≥400 | ≤200 | NBR | |||
| HS EPAC | A,C | Chemical Resistant -30 °C ~+125*C | ≥15 | ≥400 | ≤250 | CR/IIR | |||
| HS EPT | T1/T2/T3/T4 | Heat Resistant +100 °C ~+300°C | ≥15 | ≥400 | ≤200 | SBR/EPDM | |||